Hydrogen (H) is the most harmful element in general steel such as A588 Gr K structural steel plate. Hydrogen dissolved in steel will cause hydrogen embrittlement, white spots and other defects. Hydrogen, like oxygen and nitrogen, has very little solubility in solid steel. It dissolves into liquid steel at high temperature, and accumulates in the structure without time to escape when cooling, forming high-pressure micro pores, which greatly reduce the plasticity, toughness and fatigue strength of steel, and even cause cracks and brittle fracture in severe cases. "Hydrogen embrittlement" mainly occurs in martensitic steel, but not very prominent in ferrite steel, and generally increases with hardness and carbon content.
A588 Gr K structural steel plate Flaw detection standard: our steel plates can be produced and inspected in accordance with China (JB4730, GB/T2970), the United States (A435, A577, A588), Japan (JIS G0801, JIS G0901), Germany (SEL072), Britain (BS5996), France (NFS04-305) and other domestic and foreign flaw detection standards. Delivery status: according to the user's requirements, A588 Gr K structural steel plate can be delivered in hot rolling, normalizing, tempering, normalizing and tempering, quenching and tempering, etc.
In view of the characteristics of container transportation, such as high added value, low cargo damage and short time, our company takes more consideration of port collection and distribution conditions, port facilities, flight density and route coverage when choosing ports. For the convenience of customers, as well as the safety of goods.
A588 Gr K structural steel plate Shanghai inventory: 12.9*2987*10384, 15*2200*10270, 14*1950*10600, 320*2200*4250, 32*2500*6000, 14*2200*10030, 65*3010*8230, 16*2100*10650, 36*2200*12000, 12.9*2987*10384, 14*1950*10900, 25*2500*12000, 15*2200*10270, 20*2620*11800, 14*1950*10450, 30*2200*12000, 14*2200*10030, 20.9*2851*7000, 20*2933*7300, 14*1950*10500, 50*2200*12000, 31.9*2920*9420, 20*2933*7300.