Looking to the future, our company will make its main business more competitive while carrying out diversified, extensive, green and harmonious development modes, so as to be the most competitive A572 Gr 60 ms steel coil producer in the world as well as a worldwide first-class enterprise. With ten years cooperation with these big mills, now we are the agent of super stainless steel mills in China.
Manganese steel plates emerge as a profitable solution to diverse kinds of acid attacks. These have qualities surpassing an ordinary steel plate. Neither fully austenitic nor ferritic, these plates A572 Gr 60 ms steel coil provide boosted resistance to chloride stress corrosion cracking, which the 300 series stainless steel plates are susceptible to. 22% Chromium allows these plates to withstand Sulphuric and Hydrochloric acid attacks, whereas Molybdenum (up to 3%) avoids crevice and pitting corrosion.
The company adheres to the people-oriented concept and takes "learning, sharing, gratitude, integrity, respect and responsibility" as the enterprise values. Advanced equipment, scientific standardized management, strict quality assurance system and high-quality team are the core competitiveness of the company. The company will continue to provide customers with A572 Gr 60 ms steel coil high-quality, timely and perfect steel products and services under the guidance of the mission of "striving for perfection to meet customer needs".
The effect of nitrogen (N) on the properties of A572 Gr 60 ms steel coil and so on steel is similar to that of carbon and phosphorus. With the increase of nitrogen content, the strength of steel can be significantly improved, especially the plasticity, especially toughness, and the weldability will be decreased, and the cold brittleness will be intensified. At the same time, aging tendency, cold brittleness and hot brittleness will be increased, which will damage the weldability and cold bending property of steel. Therefore, the nitrogen content in A572 Gr 60 ms steel coil and so on steel should be reduced and limited as much as possible. Generally, nitrogen content should not be higher than 0.018%.