The company's A514 grade J alloy steel plate steel products are sold all over the world with high quality and low price. We can process and cut all kinds of special-shaped parts according to your requirements, or we can set and roll futures of all kinds of material specifications according to your requirements, with fast delivery time. We sincerely welcome new and old customers from all walks of life to contact us for A514 grade J alloy steel plate business negotiation.
A514 grade J alloy steel plate surface cracks refer to the linear cracks on the surface of A514 grade J alloy steel plate, which should generally be the same as the forging or rolling direction. Formation reason: it is mainly due to the hairline, hot crack and cold crack caused by surface over burning, decarburization, looseness, deformation and excessive internal stress during processing (forging, rolling, heat treatment, quenching and tempering), as well as the high content of sulfur and phosphorus impurities on the surface. Inspection method: A514 grade J alloy steel plate surface cracks can be detected by naked eye observation, acid pickling, magnetic particle inspection, coloring inspection and metallographic method.
Normalizing is a special case of annealing, the effect is similar to annealing, but the microstructure obtained by normalizing is finer. For low or medium carbon steel, normalizing can improve hardness and machinability. For A514 grade J alloy steel plate medium carbon steel and low alloy steel, normalizing can refine grain and uniform structure and reduce hardness. For high carbon steel and high alloy steel, normalizing can eliminate the network carbide produced by forging and improve the homogeneity of the preparation heat treatment structure.
Q345E steel plate is a low-alloy high-strength steel plate with good low-temperature impact performance. The steel grade is composed of three parts: Q (Qufu in Chinese spelling) representing yield strength, yield strength value, and quality grade symbol. A514 grade J alloy steel plate, Among them: Q represents the yield strength; 345 represents the yield strength value, unit MPa; E represents the grade (passed -40 degrees impact test).