Our company's A709 grade HPS50W bridge steel plate power boilers, heating furnaces of double bars, double high lines and medium and thick plates all adopt heat storage technology, which can fully use blast furnace gas; the ladle baking, Maerz active lime kiln and medium and thick plate heat treatment furnace all burn converter gas, which can improve the A709 grade HPS50W bridge steel plate utilization rate of secondary energy and realize negative energy steelmaking in steelmaking process.
The company specializes in steel plate cutting, steel plate processing and wide thick plate, hot rolling coil. The company possesses advanced CNC steel plate cutting processing equipment, first-class technical personnel, supporting marketing and after-sales service system. Steel plate cutting parts are mainly used in mechanical manufacturing, shipbuilding, steel structure and mold processing industries, and we can provide A709 grade HPS50W bridge steel plate, finished products and semi-finished products processing according to the needs of users.
Different form A709 grade HPS50W bridge steel plate, room temperature and medium temperature boiler steel shall have those advantages:Higher room temperature strength;Good impact toughness and low notch sensitivity;As the drum and other parts require a lot of cold deformation during processing, room temperature and medium temperature boiler steel must have good aging toughness;Good processing technology and welding performance;Good macrostructure, etc.
Phosphorus is a very harmful element in A709 grade HPS50W bridge steel plate steel. With the increase of phosphorus content, the strength, flexion ratio and hardness of A709 grade HPS50W bridge steel plate steel increased, but the plasticity and toughness decreased significantly. In particular, the lower the temperature, the greater the impact on plasticity and toughness, increase the cold brittleness of steel.
15Mo3 steel plate is used for boiler and high temperature pressure vessel.15Mo3 steel plate executive standard: DIN17155Delivery status of A709 grade HPS50W bridge steel plate, 15Mo3 steel plate: normalizingNormalizing temperature of 15Mo3 steel plate: 650 ~ 700 ℃Normalizing time of 15Mo3 steel plate: 1.5t-2.5t15Mo3 welding repair: welding repair can only be carried out after the approval of the purchaser.Requirements for tensile properties of 15Mo3 steel plate: tensile strength 450-600 MPa, yield strength 270 MPa.
The A709 grade HPS50W bridge steel plate pressure vessel steel plates are our featured products. We have supplied pressure vessel steel plates to tank manufactures, boiler makers, power plants and so on customers all over the world. We have online service for you at any time, welcome to contact and learn more information about pressure vessel steel, such as A709 grade HPS50W bridge steel plate ASTM A537 class 1 equivalent, 16Mo3 datasheet, Q245R material properties, Q345R material specification, P355GH properties, pressure vessel steel price, etc.
It is very important for a company to have a sound after-sales service system, which better guarantees the interests of customers and increases the reliability of the company's products in the hearts of customers. Our company has a dedicated after-sales service team and good after-sales service reputation, and has been recognized by customers over the past decades. Whenever there is problem about our A709 grade HPS50W bridge steel plate steel materials during application on the user site, our after-sales service persons will assist to find solutions at the first time.